Summary of Major Points- Flash Rust Project NSRP

NSRP Flash Rust Project Metric Table, Control of Amount

Summary of Major Points:
1.    Flash Rust is the rust that occurs from the time the waterjetting process starts to the time the water used for the waterjetting process dries.
2.    Control the quantity of Flash Rust by Project Planning
          • During Removal Process
          • As Water is drying
          • Keep the drying time to a minimum.
3. Remove excess loose Flash Rust prior to Painting

 4. Based on the subjective methods, Flash Rust is classified as
           • None
           • Light
           • Moderate
           • Heavy

The following metric table was developed by Pete Ault, Elzly Technology Corporation. Click Table to enlarge.

Table of Metrics used in Flash Rust
Table of Metrics used in Flash Rust

 

Continue reading “Summary of Major Points- Flash Rust Project NSRP”

Summary of Wipe, Swatch, and Brush Methods

Core Idea: All Methods lead to the same conclusion.


 None
 Light
 Moderate
 Heavy
Adopt the method with which you feel most comfortable and that is portable to different projects and sites.

050-swatch-hand-brush-wipe-light-flash-rust-comparison
Examples of LFR on Swatch, wipe, and Brush
051-swatch-brush-wipe-moderate-light-flash-rust-comparison
Example of MFR on swatch and brush wipe.
052-swatch-heavy-flash-rust
HFR on Swatch
053-brush-wipe-heavy-flash-rust
HFR on Brush Wipe
053-hand-wipe-heavy-flash-rust
HFR with Swatch, Brush, and Wipe

Summary of Brush Test

Summary- Brush Test:


 Brushing flash rust is quick, simple, and very reproducible.
 Adopt a standard brush and standard cloth.
 Be consistent with one swipe and in the same direction and duration.
 Practice brush strokes with even pressure
 Keep the contact area consistent.
 Cloth can be cut at the area of color transfer and placed in permanent file or scanned for color.