Archive by Author

Acknowledgements

Posted on 16. Mar, 2009 by charles frenzel.

0

Acknowledgements Many people contributed to this module.  The technical team members include: National Shipbuilding Research Program SP-3 Panel, Todd Pacific Shipyard, Detyens Shipyard, Atlantic Marine Florida LLC, Carolina Equipment and Supply Co. (CESCO), UHP Projects, and NLB Corporation. My appologies if I missed someone. There are many other factors of inspection of the substrate when [...]

Continue Reading

Pressure Sensitive Tape Test for Quantity

Posted on 16. Mar, 2009 by charles frenzel.

0

Pressure Sensitive Tape Test- for Quantity The Pressure Sensitive Tape Test described by Hempel is a modification of ISO 8502-3 (Pressure Sensitive Tape test for dust) and is not mentioned in VIS-4.  The tape test can be used as a permanent record.  If lint deposition is a concern, the project specification may require use of [...]

Continue Reading

Summary of Major Points

Summary of Major Points

Posted on 16. Mar, 2009 by charles frenzel.

0

Summary of Major Points: 1.    Flash Rust is the rust that occurs from the time the waterjetting process starts to the time the water used for the waterjetting process dries. 2.    Control the quantity of Flash Rust by Project Planning           • During Removal Process           • As Water is drying           • Keep the drying time to a minimum. 3. [...]

Continue Reading

Example of Pressure Wash on Moderate Flash Rust

Posted on 16. Mar, 2009 by charles frenzel.

0

Example of Pressure Wash on MFR: Below: the substrate is dry- but it is  darker (overall) than the original substrate. This surface is dry within 5 minutes. The standard pictures in VIS-4 do not provide these types of illustrations of pressure-washed surfaces. The upper half is not washed; the lower half has been pressure washed. [...]

Continue Reading

Pressure Washing and Excess Flash Rust

Posted on 16. Mar, 2009 by charles frenzel.

0

What Happens if there is too much Flash Rust prior to painting?  Prior to the application of paint, the substrate must meet the procurement specifications.  Typical field remediation includes:  Pressure washing  Broom brushing  Blowing off with pressurized air  Solvent cloth or dry cloth wiping  Vacuum Upon polling contractors, it appears that pressure washing is the [...]

Continue Reading

Summary of Wipe, Swatch, and Brush Methods

Posted on 15. Mar, 2009 by charles frenzel.

0

Core Idea: All Methods lead to the same conclusion.  None  Light  Moderate  Heavy Adopt the method with which you feel most comfortable and that is portable to different projects and sites.

Continue Reading

Summary of Brush Test

Posted on 15. Mar, 2009 by charles frenzel.

0

Summary- Brush Test:  Brushing flash rust is quick, simple, and very reproducible.  Adopt a standard brush and standard cloth.  Be consistent with one swipe and in the same direction and duration.  Practice brush strokes with even pressure  Keep the contact area consistent.  Cloth can be cut at the area of color transfer and placed in [...]

Continue Reading

Different Areas with Brush Test

Posted on 15. Mar, 2009 by charles frenzel.

0

Comparative results: Heavy Flash Rust formed from water coming from holes. Different section where Light, moderate, and heavy flash rust had formed in close proximity.      

Continue Reading

Example of Moderate Flash Rust on Brush

Posted on 15. Mar, 2009 by charles frenzel.

0

Example of Moderate Flash Rust on Brush:

Continue Reading